The purpose of this study was to investigate micro-morphology of the resin-dentin inter-diffusion zone using two different single-bottle self-etching dentin adhesives with and without previous acid-etching, after in vitro mechanical loading stimuli. Extracted human third molars were sectioned to obtain dentin surfaces. Two different single-bottle self-etching dentin adhesives, Futurabond U and Experimental both from VOCO, were applied following the manufacturer's instructions or after 37% phosphoric acid application. Resin-dentin interfaces were analyzed with dye assisted confocal microscopy evaluation (CLSM), including the calcium-chelation technique, xylenol orange (CLSM-XO). CLSM revealed that resin-dentin interfaces of unloaded specimens were deficiently resin-hybridized, in general. These samples showed a Rhodamine B-labeled hybrid complex and adhesive layer completely affected by fluorescein penetration (nanoleakage) through the porous resin-dentin interface, but thicker after PA-etching. Load cycling promoted an improved sealing of the resin-dentin interface at dentin, a decrease of the hybrid complex porosity, and an increment of dentin mineralization. Load cycled specimens treated with the XO technique produced a clearly outlined fluorescence due to consistent Ca-mineral deposits within the bonding interface and inside the dentinal tubules, especially when the experimental adhesive was applied.
No takes yet. Share an insight, caveat, or question.
Toledano et al. (2015) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: