This is the authors' abstract. We don't add key points for this paper.
Amorphous LaAlO3 thin films were deposited at room temperature directly on n-type and p-type Si (001) by molecular beam deposition. The dielectric properties of the stoichiometric amorphous LaAlO3 thin films deposited on silicon were determined through capacitance-voltage and current-voltage measurements. The electrical measurements indicate that the amorphous LaAlO3 thin films have a dielectric constant (K) of K=16±2. This is significantly lower than the K=24 of crystalline LaAlO3. The equivalent oxide thickness values range between 9.8 and 15.5Å for films deposited on n-type silicon with physical thicknesses of 45–75Å.