The thermal decomposition of chemically deposited SnS thin films to SnO2 films by air annealing at temperatures up to 400°C is discussed. The conversion of a 0.7 μm thick SnS thin film to an SnO2 film involves the creation of non‐stoichiometric SnS, SnS + SnS2 mixed phase and non‐stoichiometric SnO2 (i.e. SnO2 x), as concluded from X‐ray diffraction patterns, optical transmission spectra and electrical characteristics. The SnO2 thin films obtained in this manner are photoconductive, with a lowest sheet resistance (in the dark) of about 105 Ω/□ and an activation energy (Ea) of 0.1 eV for the electrical conductivity observed for the SnS films annealed at 325°C. This was found as the onset temperature for conversion of the SnS + SnS2 phase to the non‐stoichiometric SnO2 – x film. Elevation of the annealing temperature to 400°C results in an elevation of the sheet resistance to about 109 Ω/□ with the value of Ea at 1.3 eV, indicating an improvement in the degree of stoichiometry.
No takes yet. Share an insight, caveat, or question.
Nair et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: