Answers are grounded in this paper and cite their sources.
The rate of corrosion of stranded tinned‐copper cable by aqueous fluxes based on zinc and ammonium chlorides is critically related to the percentage of the latter present. Below 50% ammonium chloride, the rates for solutions of mixtures of the salts are almost as low as that for zinc chloride solution alone, where the time to destroy the tin coating and attack the underlying copper is generally of the order of 300 days or more. For compositions higher than the range 60—70% ammonium chloride, the time to attack the underlying copper falls to the order of 10 days or less, this time becoming proportionately shorter until, for ammonium chloride solution alone, it is less than 24 h. This phenomenon has been linked with migration of flux solution along the cable via the spaces between strands. Migration for solutions containing less than 50% ammonium chloride is negligible, but for higher concentrations it is appreciable. Supporting work with glass capillaries has shown that at 70% ammonium chloride, the migration is accompanied by the maximum relative enrichment in this salt. It is suggested that this migration‐enrichment is the cause of the steep increase of rate of attack at this range of composition and that attack is initiated by transported material rich in ammonium chloride.
No takes yet. Share an insight, caveat, or question.
Clarke et al. (1965) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: