This is the authors' abstract. We don't add key points for this paper.
The densification of non‐oxide ceramics like titanium boride (TiB 2 ) has always been a major challenge. The use of metallic binders to obtain a high density in liquid phase‐sintered borides is investigated and reported. However, a non‐metallic sintering additive needs to be used to obtain dense borides for high‐temperature applications. This contribution, for the first time, reports the sintering, microstructure, and properties of TiB 2 materials densified using a MoSi 2 sinter‐additive. The densification experiments were carried out using a hot‐pressing and pressureless sintering route. The binderless densification of monolithic TiB 2 to 98% theoretical density with 2–5 μm grain size was achieved by hot pressing at 1800°C for 1 h in vacuum. The addition of 10–20 wt% MoSi 2 enables us to achieve 97%–99%ρ th in the composites at 1700°C under similar hot‐pressing conditions. The densification mechanism is dominated by liquid‐phase sintering in the presence of TiSi 2 . In the pressureless sintering route, a maximum of 90%ρ th is achieved after sintering at 1900°C for 2 h in an (Ar+H 2 ) atmosphere. The hot‐pressed TiB 2 –10 wt% MoSi 2 composites exhibit high Vickers hardness (∼26–27 GPa) and modest indentation toughness (∼4–5 MPa·m 1/2 ).
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Murthy et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: