This is the authors' abstract. We don't add key points for this paper.
Supercritical fluid deposition (SCFD) of a conformal and stoichiometric Bi 4 Ti 3 O 12 (BIT) bismuth titanate film was developed in this work. It was achieved by adding a bismuth (Bi) precursor, triphenylbismuth, during the deposition of TiO 2 from titanium di(i-propoxide)bis(2,2,6,6-tetramethyl-3,5-heptanedionato). Conformal deposition with high growth rate was possible. In this system, the oxygen atom-containing ligands of the Ti precursor may have acted as an oxidant for the oxygen atom-free Bi precursor to enable deposition of Bi 2 O 3 . The effect of growth temperature was investigated for the individual depositions of TiO 2 and Bi 2 O 3 at 200–350°C. It was optimized at 300°C to minimize the generation of carbon impurity and particles. Stoichiometric BIT with a smooth surface morphology was obtained by tuning the concentrations of the Ti and Bi precursors. A uniform thickness and composition were confirmed on trenches with an aspect ratio of 7. The as-deposited BIT film on a RuO 2 underlayer, which has the same crystal structure as BIT, crystallized in the (111) and (117) orientations. The conformal, stoichiometric, smooth and crystalline BIT film grown by our SCFD method is of interest for three-dimensional structured devices, such as ferroelectric random-access memories.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Zhao et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: