A comparative investigation has been carried out on the mechanical properties and bioactivity of Bioglass-based foams, before and after applying a poly(D,L-lactic acid) (PDLLA) coating layer on the foam struts. It was found that the bioactivity of foams upon immersion in simulated body fluid (SBF) was maintained in the PDLLA-coated foams; however, the transformation kinetics in SBF of the crystalline phase (Na(2)Ca(2)Si(3)O(9)) in the foam struts to an amorphous calcium phosphate phase was retarded by PDLLA coating. The compressive and three-point bending strengths of the Bioglass-based foams were slightly improved by the PDLLA-coating, and the work-of-fracture of the foams was considerably enhanced, as indicated by stress-strain curves. Immersion in SBF for 4 weeks led to a large decrease of the mechanical strength of as-sintered foams decreased (from 0.3 to 0.03 MPa), because of the transformation of the crystalline phase to an amorphous calcium phosphate. On the other hand, the mechanical strength was well-maintained in PDLLA-coated foams after immersion in SBF for 8 weeks. This behavior was attributed to the in-situ formation of a nanocomposite PDLLA/calcium phosphate film on the strut surfaces upon immersion in SBF.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: