The surface glass‐transition temperature (T ) in monodisperse polystyrene (PS) films was examined on the basis of the temperature dependence of the lateral force at a given scanning rate. T of the PS films was found to be markedly lower than the corresponding bulk glass‐transition temperature over the entire molecular weight range (4900–1,460,000). Also, the apparent activation energy of the surface segmental motion in the PS films was 230 ± 10 kJ mol−1, significantly smaller than that for bulk PS. Finally, T measurement by lateral force microscopy was applied to binary PS mixtures with different molecular weights. On the basis of the Gordon–Taylor equation, the surface composition of the shorter component in the blend films was successfully obtained.