Increasing local pH due to oxygen reduction induced self-discharge is the main mechanism of material dissolution and capacity fade of NaTi 2 (PO 4 ) 3 electrodes in aqueous media. This problem can be strongly mitigated by ALD of a protective Al 2 O 3 layer.