Ultrafine 5.5 mol% CeO 2 —2 mol% YO 1.5 ZrO 2 powders with controllable crystallite size were synthesized by two kinds of coprecipitation methods and subsequent crystallization treatment. The amorphous gel produced by ammonia coprecipitation and hydrothermal treatment at 200°C for 3.5 h results in an ultrafine powder with a surface area of 206 m 2 /g and a crystallite size of 4.8 nm. The powder produced by urea hydrolysis and calcination exhibits a purely tetragonal phase. In addition, the powders crystallized by hydrothermal treatment exhibit high packing density and can be sintered at lower temperature (,1400°C) with nearly 100% tetragonal phase achieved.