Answers are grounded in this paper and cite their sources.
The rates of vaporization from (0001) and (101̄0) surfaces of zinc single crystals have been measured by the torsion–Langmuir method and have been compared to rates of vaporization of zinc from torsion effusion cells. A small concentration of impurities lowers the vaporization coefficient αυ for the (0001) surface to 0.7, but αυ for the (101̄0) surface of the same material and for the (0001) surface of high purity crystals are unity. The concentration of dislocations that were active in causing thermal etching of the (0001) surfaces was of the order of 105/cm3 for the samples tested. These experimental results are not in accord with the prediction of the Hirth and Pound model for metal vaporization that αυ = 13 for low index, low defect surfaces.
No takes yet. Share an insight, caveat, or question.
Mar et al. (1970) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: