Answers are grounded in this paper and cite their sources.
Synthetic hydroxyapatite (OHAp), Cas(PO.)aOH, was prepared by slow addition of phosphoric acid to a boiling Ca(OH), suspension. The solid, precipitated at a pH of about 12, was stabilized by pro longed boiling. The Ca/p ratio of the product was 1.69 0.04 and it had a specific surface area of 26 m 2 /g. Samples of OHAp were equilibrated with phosphoric acid solutions. Within the pH range studied, 5 to 7, the solubility product, (Ca)5(PO.)3(OH), was found to be 6.3 2.1 X 10 -59 at 25C. Substantial deviations of the overall dissolution reaction from OHAp stoichiometry were observed and are attributed to non stoichiometric reactions occurring at the surface. A linear dependence of excessive phosphorus on the surface with decrease in pH was found. Estimates on the extent of devia tion from stoichiometry caused by the surface reaction are given.
No takes yet. Share an insight, caveat, or question.
Avnimelech et al. (1973) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: