The elastomeric performance of the polyurethanes (PUs) is heavily dependent on controlling segment crystallinity. This study aims to develop non-crystalline flexible amorphous PUs by employing asymmetric isocyanates and multi-functional chain extenders to achieve amorphous structures. PU samples were synthesized with Hexamethylene diisocyanate (HDI) and Isophorone diisocyanate (IPDI), and chain extenders including 1,4-butanediol (BDO) and glycerol (GL). Fourier-transform infrared spectroscopy (FTIR) confirmed successful synthesis, and atomic force microscopy (AFM) revealed clear morphological differences indicating varying phase separation. Differential scanning calorimetry (DSC) and X-ray diffraction (XRD) analyses showed that IPDI-based PUs, particularly those using GL, effectively prevented crystallization in the soft segments. Mechanical testing revealed superior elongation and tensile strength in IPDI-based formulations compared to linear HDI-based samples, attributed to reduced phase separation and enhanced molecular network density.
No takes yet. Share an insight, caveat, or question.
Alizadeh et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: