Pulsed laser deposition was used to deposit thin films of calcium hydroxylapatite (Ca10(PO4)6(OH)2), or HA, on polished substrates of Ti‐6Al‐4V. Thin films of pure, crystalline HA, uncontaminated by other calcium phosphate phases, were deposited over a range of temperatures between 400 and 800°C. The HA films were polycrystalline with a preferred (001) crystallographic orientation, as determined by transmission electron microscopy and x‐ray diffraction. Adhesion of the HA films to the Ti‐6Al‐4V substrates was excellent when films were deposited at temperatures ≤600°C; in a scratch test, mean pressures of ca. 1010 Nm−2 produced conformational cracking in a film deposited at 600°C, but no decohesion from the substrates.