This is the authors' abstract. We don't add key points for this paper.
The graphitization mechanism with Ni, which is one of the most important catalysts for graphitization, involves the precipitation of carbon from the Ni. There are two possible precipitation pathways: through the C solubility gradient by cooling, and through the segregation from the intermediate carbide phase [1-5]. In this study, through in situ heating transmission electron microscopy (TEM), we present the graphitization mechanism of stacked Ni and amorphous carbon (a-C) film. Our study revealed that the graphitization started at about 450 °C during the heating process. The catalyst showed the presence of nickel carbide (Ni3C) phase, in which C occupies the octahedral interstitial site of Ni. This phase transition caused lattice distortion of the Ni crystal. The real-time atomic resolution TEM imaging and the results of the Fast Fourier Transform (FFT) analysis confirmed the existence of these two phases. The intermediate phase became unstable at temperatures above 450 °C. Above this temperature, the carbide phase dissociates into Ni and C, which is a source of carbon even during the heating process [6]. Graphitization via the carbide mechanism does not occur layer-by-layer, but rather multiple layers grow simultaneously. Morphological analysis of the grown film showed that graphitization occurred at Ni surface rather than a-C interface [1]. Our study contributes to the understanding of catalytic reactions at the nanoscale through real-time analysis. This can aid in designing catalysts with desired structures [8]. (a) During the in situ TEM experiment, a single TEM image of the reaction surface was captured at atomic resolution. The image shows the d spacing on octahedral structure of each phase for clarity and the corresponding FFT of each phase. (scale bar = 1 nm) (b) lattice structure of Ni3C(211¯)and Ni (110) and the distance between Ni atoms [1, 7]. 1 sec interval time-elapsed images from in situ heating TEM experiment. The graphene layers grown on the catalyst surface are marked by the red dotted lines. (scale bar = 5 nm)
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: