Answers are grounded in this paper and cite their sources.
Ceramics in the solid solution system, (1 − x )Ba 0.8 Ca 0.2 TiO 3 – x Bi(Mg 0.5 Ti 0.5 )O 3 , were prepared by a conventional mixed oxide route. Single‐phase perovskite‐type X‐ray diffraction patterns were observed for compositions x < 0.6. A change from tetragonal to single‐phase cubic X‐ray patterns occurred at x ≥ 0.1. Dielectric measurements indicated relaxor behavior for x ≥ 0.1. Increasing the Bi(Mg 0.5 Ti 0.5 )O 3 content improved the temperature sensitivity of relative permittivity ϵ r at high temperatures. At x = 0.5, a near‐plateau relative permittivity, 835 ± 40, extended across the temperature range, 65°C–550°C; the permittivity increased at x = 0.6 to 2170 ± 100 for temperatures 160°C–400°C (1 kHz). The corresponding loss tangent, tanδ, was ≤0.025 for temperatures between 100°C and 430°C for composition x = 0.5; at x = 0.6, losses increased sharply at >300°C. Comparisons of dielectric properties with other materials proposed for high‐temperature capacitor applications suggest that (1 − x )Ba 0.8 Ca 0.2 TiO 3 – x Bi(Mg 0.5 Ti 0.5 )O 3 ceramics are a promising base material for further development.
No takes yet. Share an insight, caveat, or question.
Zeb et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: