This is the authors' abstract. We don't add key points for this paper.
This study investigates the photodegradation of methyl orange dye using the Pd/NiFe2O4/chitosan nanobiocatalyst under sunlight irradiation. The characterization of Pd/NiFe2O4/chitosan was examined using FESEM, TEM, and XRD analyses, which confirms its successful synthesis and desirable morphological properties. The key parameters, which including the initial concentration of dye (5–20 ppm), solution pH (5–10), and catalyst amount (5–25 mg) were evaluated. The optimal conditions were determined to be an initial dye concentration of 5 ppm, a pH of 9, and a photocatalyst amount of 15 mg, resulting in a degradation efficiency of 96% within 60 min. Kinetic studies showed that the degradation process follows pseudo-first-order kinetics. Scavenger experiments indicated that superoxide radicals are primarily responsible for the degradation mechanism, while hydroxyl radicals and holes (h+) act as species with lower activity. The photocatalyst exhibited excellent stability and reusability, maintaining high efficiency over six consecutive cycles without a noticeable decrease in performance.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Panahimehr et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: