The structure and chemical environment of Cu in Cu/CeO 2 catalysts synthesized by the solution combustion method have been investigated by X-ray diffraction (XRD), transmission electron microscopy (TEM), electron paramagnetic resonance (EPR) spectroscopy, X-ray photoelectron spectroscopy (XPS), cyclic voltammetry (CV), and extended X-ray fine structure (EXAFS) spectroscopy. High-resolution XRD studies of 3 and 5 atom % Cu/CeO 2 do not show CuO lines in their respective patterns. The structure could be refined for the composition Ce 1 - x Cu x O 2 - δ ( x = 0.03 and 0.05; δ ∼ 0.13 and 0.16) in the fluorite structure with 5−8% oxide ion vacancy. High-resolution TEM did not show CuO particles in 5 atom % Cu/CeO 2 . EPR as well as XPS studies confirm the presence of Cu 2+ species in the CeO 2 matrix. Redox potentials of Cu species in the CeO 2 matrix are lower than those in CuO. EXAFS investigations of these catalysts show an average coordination number of 3 around the Cu 2+ ion in the first shell at a distance of 1.96 Å, indicating the O 2 - ion vacancy around the Cu 2+ ion. The Cu−O bond length also decreases compared to that in CuO. The second and third shell around the Cu 2+ ion in the catalysts are attributed to −Cu 2+ −O 2 - −Cu 2+ − at 2.92 Å and −Cu 2+ −O 2 - −Ce 4+ − at the distance of 3.15 Å, respectively. The present results provide direct evidence for the formation of a Ce 1 - x Cu x O 2 - δ type of solid solution phase having −□−Cu 2+ −O−Ce 4+ − kind of linkages.
No takes yet. Share an insight, caveat, or question.
Bera et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: