The creep behaviour of high-density silicon carbide has been examined under four-point transverse bending in air at temperatures from 1000 to 1300°C. Stresses in the range 0·207 GN m −2 (30 000 Ib in −2 ) to 0·496 GN m −2 (72000 lb in −2 ) were applied. In tests lasting up to 3·6 Msec (1000 h) the creep strain ( ϵ p ) increased with time ( t ) as ϵ p = At k where k was between 0·2 and 0·5. The dependence of A on stress (σ) and absolute temperature ( T ) was found to be A ∝ σ n exp(- Q/RT ) with n between 1 and 2 and Q ∼230 kJ mole −1 (55 kcal mole −1 ). These results are compared with estimates of creep in SiC obtained by extrapolation of steady-state creep data from higher temperatures.