Owing to stringent service conditions, nickel-based superalloys must meet exceptionally high surface quality standards. After cold rolling, these alloys can blacken during annealing, affecting appearance and performance. The surface-element distribution of GH4169 alloy annealed under hydrogen protection was analyzed via XPS, and reaction free-energy changes were calculated using thermodynamic software. The blackened surface contained oxides and carbides, primarily Cr2O3, Cr(OH)3, TiO2, Nb2O5, NbC, and free carbon. Residual water vapor in the protective hydrogen gas and rolling-oil remnants generated C, CO2, CO, and H2O, which then reacted with the alloy during high-temperature annealing to form a blackened layer. The selective oxidation of Cr, Nb, and Ti, along with the inward diffusion of carbon, leads to the compositional differences observed in the blackened layer. Lowering the protective gas dew point, improving rolling oil, and effective degreasing eliminated blackening.
No takes yet. Share an insight, caveat, or question.
Yang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: