We found that excess water molecules and hydrocarbons, existing in the bonding interface and thought to cause voids, were absorbed in the damaged area of the amorphous layer formed on the surface of the wafer upon direct bonding of silicon wafers, thus making it possible to suppress void formation with relatively low heat-treatment temperature of 600° C for 3 h.