This is the authors' abstract. We don't add key points for this paper.
Spinel cathode materials consisting of LiMn2 O4 @LiNi0.5 Mn1.5 O4 hollow microspheres have been synthesized by a facile solution-phase coating and subsequent solid-phase lithiation route in an atmosphere of air. When used as the cathode of lithium-ion batteries, the double-shell LiMn2 O4 @LiNi0.5 Mn1.5 O4 hollow microspheres thus obtained show a high specific capacity of 120 mA h g(-1) at 1 C rate, and excellent rate capability (90 mAhg(-1) at 10 C) over the range of 3.5-5 V versus Li/Li(+) with a retention of 95 % over 500 cycles.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: