Answers are grounded in this paper and cite their sources.
Fiber structure development of the continuous neck-drawing process of Nylon 6 (poly ε-caprolactam) fibers was investigated by in situ wide-angle X-ray diffraction and small-angle X-ray scattering measurements using the ultrahigh luminance synchrotron radiation of SPring-8. Feed speeds of 4 and 25 m/min were used with time resolutions of 1.7 and 0.43 ms, respectively. The estimated temperature of the running fiber jumped from 90 to 140150 ̊C with necking, and reached a maximum temperature of about 185 ̊C. The pseudohexagonal phase was oriented along the fiber axis by necking, and transformed to the α'-crystal from 20 to 110 ms after necking. The ά-crystal transformed to the α-crystal below 130 ̊C. The low-oriented long-period structure of the as-spun fiber disappeared by necking, and a higher oriented long-period structure was reconstructed within 10 ms after necking. The 7.8 nm long-period of the as-spun fiber increased to 9.5 nm with the reconstruction.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: