Non-woven hybrid meshes based on poly( l -lactide- co - d,l -lactide) ( dl -PLA) and β-tricalcium phosphate (β-TCP) were fabricated and comprehensively characterized. Stock suspensions of β-TCP powder in dl -PLA acetone solutions were used for the electrospinning process. Structure, morphology and thermal properties of the electrospun samples were investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The electrospun hybrid materials show a micro-composite structure, and a morphology characterized by a three-dimensional porous fibrous mesh with randomly distributed fibers possessing average fiber diameters between 680 and 970 nm, uniform thickness along the fibers and beads structure only for higher β-TCP concentration electrospun samples. Both pure PLA and hybrid non-woven meshes exhibit a good thermal stability and a continuous degradation in simulated body fluid medium. A live/dead staining viability assay using MC3T3-E1 preosteoblasts reveals the excellent cytocompatibility of the fabricated non-wovens. Enhanced alkaline phosphatase (AP) activity of MC3T3-E1 cells during culture on the dl -PLA and the composite non-woven meshes demonstrates their potential for applications in hard tissue repair.
No takes yet. Share an insight, caveat, or question.
Tammaro et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: