Microstructure evolution of a low hard segment (<10 mol %) thermoplastic polyurethane (LHS-TPU) has been followed by in-situ wide-angle X-ray (WAX) and small-angle X-ray scattering (SAX) with a focus on elucidating peculiar microstructural changes during uniaxial deformation (λ = 1−3.5). For the LHS-TPU, the hard segments, due to their low content and chemical structure, do not crystallize but form glassy regions that act as physical cross-links. Two types of soft segment crystallites are resolved upon elongation via DSC, SAX, and WAX experiments. Phase I consists of a small amount of initial crystallites (<2%) that function similar to conventional PU hard segment domains, deforming at small uniaxial strains (λ = 1−2) to a chevron-type morphology, which exhibit equatorial 4-point patterns in SAX. Phase II evolves at higher deformations (λ > 2) due to strain-induced crystallization. Phase II exhibits a conventional meridional 2-point pattern along the deformation direction with lamellar crystallites aligning in the plane normal to the deformation. WAX, SAX, and DSC confirm that both phases coexist over a small strain window (λ = 1.9−2.5), demonstrating the independent nature of the two crystalline phases. These findings indicate that the LHS-TPU in this study is similar to poly(butylene adipate) (PBA) in its morphological and structural behavior. This is further substantiated by NMR, which reveals that the LHS-TPU consists of 90% soft segments, which are identified as PBA via crystal structure analysis of a highly aligned fiber. The soft segments in the LHS-TPU dominate the morphology and the X-ray patterns upon deformation.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Koerner et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: