Answers are grounded in this paper and cite their sources.
0.0001)among the four groups and Duncan's multiple range test showed that microwave cured + fibers significantly higher transverse strength followed by heat cured +fibers, microwave alone, while heat alone shows significantly lowest transverse strength. Residual monomer test: Analysis of variance(ANOVA) for the four groups from the first day of immersion in water until 7th day shows that there are significant differences between the four groups in the all six days except the 7th day shows that there are no significant differences among the four groups for the level of the residual monomer. CONCLUSIONS: Microwave cured acrylic resin with glass fibers have signifi-cantly higher transverse strength than that of acrylic resin cured by water bath, also microwave cured acrylic resin have significantly lower residual monomer content from the 1st day of immersion when compared to that of water bath which show the same level of residual monomer at the 7th day of im-mersion]]>
No takes yet. Share an insight, caveat, or question.
Hasan et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: