Answers are grounded in this paper and cite their sources.
Cordierite ceramics were prepared by a solid-state reaction method using iron tailings, light-burned magnesite tailings powder and calcined alumina as raw materials. The effects of sintering temperature and MgO/ Al_2{O_3} ratio on the microstructure and properties (thermal and mechanical) of the materials were systematically investigated. The results showed that at the sintering temperature of 1180°C and the MgO/ Al_2{O_3} ratio of 1, the main crystalline phase of the sample was α-cordierite (indialite), with spinel as the secondary phase. With increasing sintering temperature, the bulk density increased, the apparent porosity decreased, the room-temperature flexural strength first increased and then decreased, and the thermal expansion coefficient (20-800°C) first decreased and then increased. Optimal overall performance was achieved at the sintering temperature of 1180°C. Under this condition, the bulk density was 2.59 g/ cm³ , the apparent porosity was 4.77%, the roomtemperature flexural strength was 85.17MPa and the thermal expansion coefficient was 4.09 × 10⁻⁶ ° C⁻¹ .
No takes yet. Share an insight, caveat, or question.
Gao et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: