It is demonstrated by in situ IR spectroscopy that, in methanol conversion on ZrO 2 and 5% Cu/ZrO 2 catalysts, methoxy groups are present on the catalyst surface, which result from O-H or C-O bond breaking in the methanol molecule. Two types of formate complexes, localized on ZrO 2 and CuO, are also observed. The formate complexes form via the oxidative conversion of the methoxy groups. There are two types of linear methoxy groups. First-type linear methoxy groups condense with the formate complex located on CuO to yield methyl formate and then CO and H 2 . Second-type methoxy groups appear as intermediate products in the formation of dimethyl ether. The main hydrogen formation reactions are the recombination of hydrogen atoms (which result from the interconversion of surface complexes) on copper clusters and the decomposition of methyl formate. The source of CO 2 in the gas phase is the formate complex, and the source of CO is methyl formate. The effect of water vapor and oxygen the surface reactions and product formation is discussed.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Матышак et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: