PURPOSE: To investigate the shear bond strength (SBS) of various primer/resin cement systems to monolithic zirconia under different levels of storage. MATERIALS AND METHODS: ). The samples were divided into three groups (n = 24) according to primer/cement system: Z-PRIME Plus/DUO-LINK (Bisco); Clearfil Ceramic Primer Plus/PANAVIA SA (Kuraray); and Single Bond Universal Adhesive/RelyX Ultimate (3M ESPE). After bonding was completed, each group was divided into two subgroups (n = 12) under different levels of 24-hour storage and thermocycling. The specimens were embedded in acrylic molds, and SBS tests were conducted. Modes of failure were also evaluated. The data were analyzed using one- and two-way analysis of variance (ANOVA) and Tukey Honest Significant Difference test. Significance was set at P < .05. RESULTS: The highest and lowest SBS values were observed in the Kuraray (12.52 ± 1.34 MPa) and Bisco (5.32 ± 0.54 MPa) systems, respectively, in the thermocycled groups (P < .05). Similarly, in short-term storage groups, Kuraray had the highest (16.47 ± 1.5 MPa) and Bisco the lowest (7.43 ± 1.06 MPa) SBS values (P < .05). Regardless of adhesive system used, thermocycling significantly decreased the SBS of all cement groups (P < .05). Of the failures, 49% were adhesive, 45% were mixed, and 6% were cohesive. CONCLUSION: A methacryloyloxydecyl dihydrogen phosphate-containing resin cement is recommended to provide a durable bond for monolithic zirconia.
No takes yet. Share an insight, caveat, or question.
Özkurt‐Kayahan et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: