Low temperature (⩽450°C) deposition of single‐crystal GaAs using a new plasma‐enhanced MO‐CVD technique is reported. In this technique, plasma is created by a dc potential and the substrate is not directly exposed to the plasma. Deposition of GaAs was achieved at extremely low plasma power (0.3–0.5 W/cm 2 ) using trimethylgallium (TMGa) and arsine (or trimethylarsenic) reactants. The resulting epitaxial films show excellent surface morphology and thickness uniformity over a large area substrate. A linear dependence of growth rate upon TMGa concentration was observed with a typical growth rate of 0.1 μm/min for a TMGa flow rate of 15 ml/min. Undoped films were found to be n‐type with a room temperature mobility in the range of 5200 cm 2 V −1 · s −1 . Measurements on Schottky barrier devices fabricated on n/n + layers show uniform impurity doping profiles. Temperature dependence of the diode capacitance indicates a density of deep trapping centers as low as 6.2 × 10 13 cm − 3 .
No takes yet. Share an insight, caveat, or question.
Pande et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: