Answers are grounded in this paper and cite their sources.
Poly (lactic acid) – b – poly (ethylene glycol) (PLA-b-PEG) co-polymers with block lengths of 1000–750, 5000–1000, 1000–5000, and bulk PEG were added to PLA electrospinning dopes to create hydrophilic but non-water soluble nanofibers. PLA-b-PEG block lengths strongly affected the total amount of PEG that could be incorporated, as well as spinnability and fiber morphology. Solutions containing >1% w/w of the lowest molecular weight co-polymer PLA (1000) – b – PEG (750) formed an unspinnable, cloudy gel. Addition of the PLA (5000) – b – PEG (1000) to the base spinning solution influenced fiber diameters and spinnability in the same manner as simply increasing PLA concentration in the spinning dope. Addition of PLA (1000) – b – PEG (5000) resulted in decreased fiber diameters, and allowed for the highest overall co-polymer loading. In final fiber formulations, maximums of 0.9, 2.9 and 9.3 wt% PEG could be achieved using the PLA-b-PEG 1000–750, 5000–1000 and 1000–5000 respectively. PEG (M W = 3350 g/mol) homopolymer was added to the spinning dopes to prepare fibers with 1.0 and 5.0 wt% PEG. The resulting fibers had non-uniform morphology and more variable diameter size than occurred with the addition of PEG in block co-polymer form. Water absorbance by electrospun nonwoven fabrics increased by four times over the control PLA with the addition of 1.0 wt% PEG, and by eighteen times with the addition of 9.3 wt% PEG with the block co-polymers. At similar overall PEG loadings, the addition of PLA-b-PEG resulted in a two to four fold increase in water wicking over the addition of PEG homopolymer.
No takes yet. Share an insight, caveat, or question.
Hendrick et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: