The strain state of metal oxides Pr2O3, Y2O3 and Sc2O3 used as buffer material in different heteroepitaxially grown semiconductor-oxide-Si(1 1 1) layer stacks was studied by x-ray diffraction techniques at room temperature (RT) and near the growth temperature of 625 °C. A broad spectrum of different strain states was found depending on preparation conditions, layer combination and layer thickness. Pr2O3 behaves differently from the other two investigated oxides as it grows in a hexagonal phase on Si(1 1 1) and must be transformed into the stable cubic phase by annealing processes. This transformation is accompanied by the creation of an amorphous silicate interface layer that leads to a decoupling of substrate and oxide lattices and finally to a partial relaxation of the cub-Pr2O3 layer only. High-temperature measurements demonstrate that there exists a measurable difference between the strain state at RT, where x-ray measurements are typically performed, and at growth temperature. The coefficient of thermal expansion of different metal oxides was measured in thin film structures for the first time. These coefficients are significantly higher compared with that of Si, which leads to an additional tensile strain component when the samples are cooled down to RT.
No takes yet. Share an insight, caveat, or question.
Zaumseil et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: