The UV optical absorption edge of pure PbWO4 (PWO) and a series of La3+-doped PbWO4 crystals was measured at room temperature. Parameters, including the energy gap Eg and the energy of phonon Ep involved in the indirect transition, were calculated, and the dependence of the transition on impurities instead of phonons in heavily doped PWO:La crystals is presented. The shift of the absorption edge to higher energy observed in the case of doping at low concentration ( 1600 ppm) are explained by the combined effects of ion polarization and localized defect energy level. FT-IR spectra of the WO4 tetrahedron confirmed the coexistence of interstitial oxygen and Pb vacancies to keep the charge balance in heavily doped PWO:La crystals.