In the context of sustainable materials for outdoor applications, the use of bio-based and biodegradable composites reinforced with agro-industrial waste represents a promising strategy. However, exposure to sunlight and oxygen can lead to photo-oxidation, potentially compromising both performance and biodegradability. In this study, Mater-Bi (MB) was compounded with 10 and 20 wt% grape pomace (GP), a by-product rich in polyphenols, and the resulting biocomposites were subjected to accelerated aging. The impact of photo-oxidation was evaluated through rheological, thermal, and mechanical analyses, alongside biodegradation tests in soil. The results revealed that while neat MB undergoes significant degradation upon aging, the GP-filled composites exhibited better resistance to photo-oxidative damage. Importantly, the biodegradation behaviour of the aged samples was also investigated, highlighting how prior oxidative degradation influences the subsequent disintegration of the material in a natural environment. The findings underscore the importance of assessing the end-of-life performance of biocomposites after environmental weathering, to ensure their sustainability under real-life outdoor conditions.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Rapisarda et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: