The shortage of lithium resources and the accumulation of retired batteries are strategic issues that need to be addressed urgently. Here, we propose an innovative and efficient strategy for the preferential extraction of Li +, followed by the sequential recovery of Mn 2+ and Co 2+, utilizing GIS zeolite from battery leachate. Li + ions were preferentially exchanged, achieving a 95% recovery rate at 0 °C; subsequently, 94% of Mn 2+ and 97% of Co 2+ were recovered by increasing the temperature to 40 and 60 °C; meanwhile, 90% of Ni 2+ remains in solution. The fastest kinetic rate of Li + in GIS zeolite and its efficient extraction at low temperatures were verified through ion exchange processes; at higher temperatures, the adsorption capacity and selectivity of GIS zeolite for Co 2+ and Mn 2+ increased. We found the diffusion rate of Li + in GIS zeolite to be over 2.5 times faster than that of Mn 2+, Co 2+, and Ni 2+, which all have the same rate by molecular dynamics simulations. The ion exchange of Mn 2+, Co 2+, and Ni 2+ was an endothermic reaction, with the Δ H 0 and Δ G 0 following the order Mn 2+ < Co 2+ < Ni 2+ by thermodynamic calculations. The regeneration ability of GIS zeolite indicated its promising industrial application prospects.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: