Inorganic electron-selective layers (ESLs) are fabricated at extremely low temperatures of 70°C or even 25°C by a simple solution route. This is of great significance because the attained PCEs confirm the feasibility of room-temperature coating of inorganic amorphous ESLs through a solution method for the first time.