Answers are grounded in this paper and cite their sources.
EXAFS and XANES measurements are made for (Bi 2 O 3 –Y 2 O 3 ) system, (Bi 2 O 3 ) 0.75 (Y 2 O 3 ) 0.25 at 300 K and (Bi 2 O 3 ) 0.6 (Y 2 O 3 ) 0.4 at 60 K and 300 K, to elucidate their defect structure and the glass-like behaviors at low temperatures. In both ceramics the larger chemical shift of Y K-edge to lower energy measured from that of Y 2 O 3 is observed as compared with that of Bi L 3 -edge measured from that of Bi 2 O 3 . Small coordination number of oxygen around Y ion is also obtained by curve-fitting analysis of EXAFS for these ceramics. The results imply that oxygen defect mostly concentrates around dopant yttrium cation preserving charge balance with each other. To elucidate the glass-like behavior at low temperatures (below 12 K), schematic microscopic model of the defect structure is presented based on the data obtained here.
No takes yet. Share an insight, caveat, or question.
Kamijo et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: