Purpose: This study was conducted to evaluate the effect of adding nano-zirconia with different concentrations on the flexural and impact strength of microwaved and heat cured acrylic resin. Materials and Methods: The silanized nano-ZrO2 particles (nano-zirconia) were added to PMMA powder for both heat polymerized and microwaved acrylic resin. A total of 160 specimens were prepared from both types of acrylic resin (n=80). For both types of acrylic resin, specimens for each strength test were subdivided into 4 subgroups (n=10): a control group (with no fillers) and three reinforced groups with 3 concentrations (3%, 5% and 7%) wt. % of nano-ZrO2 fillers. Flexural strength was measured using an Instron mechanical testing machine and impact strength was measured by Charpy tester. Results: For the heat cured resin 3% nano-zirconia showed the highest mean fl exural strength value followed by 5 % nano-zirconia. For the microwaved acrylic resin, 3% nano-zirconia showed the highest mean flexural strength value while 5% and 7% led to decrease in the flexural strength value. For the impact strength results, increasing nano-zirconia percentage led to decrease the impact strength for both types of acrylic resin. Conclusions: The incorporation of 3% and 5% nano-zirconia into heat cured acrylic resin improved its fl exural strength but 7% of nano-zirconia addition had a deteriorating effect on the flexural strength of both types of resin investigated. Moreover, the addition of nano-zirconia to both types of acrylic resin had a negative effect on their impact strength.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Eid et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: