The influence of chloride ion concentration on the passivation film and corrosion product film of martensitic stainless steels (SS) (13% Cr, modified 13% Cr-1% Mo, modified 13% Cr-2% Mo, and 15% Cr SS) have been investigated using immersion tests and electrochemical measurements in sweet environments at temperatures of 150°C and 180°C in the presence of carbon dioxide (CO2). The corrosion rate of conventional 13% Cr SS was found to increase with increasing chloride ion concentration at 150°C. However, the corrosion rates of modified 13% Cr SS and 15% Cr SS were independent of the chloride ion concentration at 150°C. The corrosion rates of modified 13% Cr SS increased with increasing chloride ion concentration above 1,000 ppm at 180°C. The corrosion rate of 15% Cr SS slightly increased at high chloride ion concentration at 180°C. Chromium-enriched corrosion product films were produced on all alloys considered, except for 15% Cr SS, at 180°C. A passivation film was maintained for 15% Cr SS at 180°C. In addition, the pitting corrosion behaviors were investigated by potentiodynamic polarization curves and open-circuit potential measurements. The behavior of the current density of anodic curves corresponded to the immersion test results. Pitting corrosion on modified 13% Cr-2% Mo SS is considered to repassivate because of low potential compared with pitting potential.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Sunaba et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: