Answers are grounded in this paper and cite their sources.
New Nb/sub 3/Sn conductors with excellent high-field performance have been fabricated using Ta-Sn powder as a core material. The powder was easily synthesized by the melt diffusion reaction between Ta and Sn powders. The Ta-Sn powder was encased in a Nb or Nb-Ta alloy sheath to form a composite. The composite was fabricated into tape and wire specimens without intermediate annealing. The specimens were then reacted at 800-925/spl deg/C in vacuum. After the reaction a thick Nb/sub 3/Sn layer, several tens of micrometers in thickness, is formed between the sheath and the core. No void is formed in the core after the reaction. Ta is incorporated into the Nb/sub 3/Sn layer from both the core and the Nb-Ta sheath. The J/sub c/ of the Nb/sub 3/Sn layer reaches 5 /spl times/10/sup 4/ A/cm/sup 2/ at 23 T and 4.2 K. The tape specimens show large critical current at 23 T due to the large thickness of the Nb/sub 3/Sn layer. The optimum reaction temperature can be decreased by the small amount of Cu addition.
No takes yet. Share an insight, caveat, or question.
Tachikawa et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: