An anomalous behavior—a change in polarity with the passage of time in the bulk heterojunction poly(3-hexylthiophene) (P3HT):6,6-phenylC61 butyric acid methyl ester (PCBM) organic solar cells—is reported here. This work is a continuation of our previous work where the initial degradation of the organic solar cells, freshly prepared up to 4 h, was mainly due to domain formation in the active layer. With the passage of time, the activity at the interfaces starts becoming significant. A decrease of V OC and J SC , leading to a change in polarity, has been reported and explained up to 300 h after fabrication.