Answers are grounded in this paper and cite their sources.
In vitro and in vivo bioactivity studies were performed to assess the biocompatibility of CaO-P2O5 glass-reinforced hydroxyapatite (GR-HA) composites. The ability to form an apatite layer by soaking in simulated body fluid (SBF) was examined and surfaces were characterized using FTIR reflection and thin-film X-ray diffraction analyses. Qualitative histology, histomorphometric measurements, and push-out testing were performed in a rabbit model for characterizing bone/implant bonding. Under the in vitro conditions using SBF, an apatite layer could not be formed on GR-HA composites within 8 weeks. Results of push-out testing showed bonding between the composites and bone, ranging from 130-145 N after 2 weeks of implantation. After the longest implantation period, 16 weeks, the GR-HA composite prepared with the higher content of CaO-P2O5 glass showed the highest bonding force, 606 +/- 45 N, compared to 459 +/- 30 N for sintered HA. Development of immature bone and modifications in the turnover of a more mature bone on the surface of GR-HA composites were similar to those on sintered HA.
No takes yet. Share an insight, caveat, or question.
Lopes et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: