This is the authors' abstract. We don't add key points for this paper.
CoSb3-based skutterudites, as a medium-temperature thermoelectric material, show excellent thermoelectric performance, but high thermal conductivity suppresses the high ZT value. Here, x% SnTe/Yb0.2(CoSb2.875Te0.125)4 samples were synthesized through vacuum melting reaction and spark plasma sintering (SPS). With increasing of SnTe content, the dispersed phase CoSb2, SnTe and CoTe2 appear successively via a selection of nucleation kinetics for 1%, 3% and 5% SnTe composited sample. Due to scattering of the dispersed phase and the solid solution distortion, lattice conductivity (κlat) of the 3% SnTe/Yb0.2(CoSb2.875Te0.125)4 sample decreases from 1.55 W m−1 K−1 to 1.19 W m−1 K−1 compared with the Yb0.2(CoSb2.875Te0.125)4 sample, which reduces by ∼22.8% at 773 K. The maximum thermoelectric merit ZT of the 3% SnTe/Yb0.2(CoSb2.875Te0.125)4 sample achieves 1.18 at 773 K.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Xin et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: