Answers are grounded in this paper and cite their sources.
The partial replacement of Ni by 30 at%Cu for the Pd40Ni40−xCuxP20 alloys was found to cause the drastic increase in the glass-forming ability as is evidenced from the decrease in the critical cooling rate for glass formation (Rc) to 1.5 K/s and the increase in the critical sample thickness for glass formation (tmax) to 40 mm. The Pd40Ni10Cu30P20 amorphous alloy exhibits the distinct glass transition, followed by the appearance of a wide supercooled liquid region (ΔTx(=Tx−Tg)) reaching 95 K and then a single-stage crystallization. The differential thermal analysis indicates that the Pd–Ni–Cu–P alloy has a single stage melting reaction at 804 K. The resulting Tg⁄Tm is measured to be as high as 0.72. Considering that the Rc, tmax, ΔTx and Tg⁄Tm are 128 K/s, about 7 mm, 63 K and 0.66, respectively, for a Pd40Ni40P20 amorphous alloy with the largest glass-forming ability in previously reported Pd-based alloys, the present new Pd–Ni–Cu–P amorphous alloy is concluded to have a much larger glass-forming ability and a higher thermal stability of the supercooled liquid. The crystallization occurs through a single stage due to the precipitation of more than four kinds of crystalline phases and hence the necessity of long-range rearrangement of the constituent elements for the progress of the precipitation seems to cause the large glass-forming ability and the high thermal stability of the supercooled liquid through the retardation of crystallization. The finding of the new Pd-based amorphous alloy with the much larger glass-forming ability is important for the future development of basic science and engineering application of amorphous alloys.
No takes yet. Share an insight, caveat, or question.
Nishiyama et al. (1996) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: