The Stellite 6-coated portion of the SS316L plug stem in the pneumatic control valve failed during service due to a combination of mechanical stress and corrosive environmental conditions. Metallurgical analysis revealed brittle intergranular fracture in the Stellite coating and in the SS316L substrate. The failure initiated with stress-induced cracking in the Stellite coating, exposing the SS316L substrate, which subsequently corroded, leading to total fracture of the plug stem. Microcracks along the grain boundaries in the Stellite coating propagated under mechanical stress, exposing the SS316L substrate to localised corrosion. The failure in the SS316L substrate was characterised by stress corrosion cracking.