Answers are grounded in this paper and cite their sources.
High‐temperature tensile deformation of paolycrystalline magnesia prepared by ( a ) single‐crystal recrystallization and ( b ) hot‐pressing, is described. Recrystallized polycrystalline magnesia goes through a brittle‐ductile transition at 1700°C (strain rate 10 −4 sec −1 ). The brittleness below 1700°C is due to a lack of slip systems and grain boundary sliding. At 1700°C grain boundary migration produces corrugations in the interface which interfere with sliding. Above 1700°C the matrix becomes sufficiently plastic through multiple slip and polygonization to accommodate any distortion. Polycrystalline specimens then neck down for completely ductile fracture. Hot‐pressed magnesia starts through a transition at 2200°C, i.e. 500°C higher. The increase is attributed to pores and impurity. Porosity is considered to promote grain boundary sliding by ( a ) providing the source for intergranular sliding, ( b ) decreasing the interfacial contact area, and ( c ) preventing grain boundary migration and corrugation. These observations confirm that high‐temperature deformation occurs by dislocation glide and climb and by grain boundary sliding and migration.
No takes yet. Share an insight, caveat, or question.
Day et al. (1966) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: