The 6‐arm star‐shaped poly(L‐lactide) (6PLL)/linear poly(D‐lactide) (1PDL) stereocomplex films were prepared by the solvent casting method. The influences of the 6PLL/1PDL blend ratios (75/25, 50/50, and 25/75 w/w) and 1PDL molecular weights (15,000, 30,000, and 60,000 g/mol) on the thermal and mechanical properties of the stereocomplex films were investigated. The 6PLL and 1PDLs had a single melting temperature ( T m ) of homocrystallites at 174°C and 167°C, respectively. The 6PLL/1PDL blends had two T m s: a lower T m of homocrystallites (160–173°C) and a higher T m of stereocomplex crystallites (219–228°C). The stereocomplex crystallinity and mechanical properties of the 6PLL/1PDL blend films were higher than those of 6PLL and 1PDL and were the highest in the 50/50 (w/w) blend ratio. However, the stereocomplex crystallinity of the 50/50 (w/w) 6PLL/1PDL blend films decreased and the mechanical properties increased as the molecular weight of 1PDL increased.
No takes yet. Share an insight, caveat, or question.
Cheerarot et al. (2015) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: