Answers are grounded in this paper and cite their sources.
Beryllium-magnesium aluminate (Be 0.1 Mg 0.9 Al 2 O 4 and Be 0.2 Mg 0.8 Al 2 O 4 ) nanoparticles are synthesized by a coprecipitation method and sintered using Spark Plasma Sintering (SPS) to achieve near full density ceramics with grain sizes at the nanoscale. The sintered nanoceramics display grain sizes ranging from 14 to 33 nm, which are analyzed for optical transmission, Vickers hardness, and cation site inversion. When compared to Be-free MgAl 2 O 4 nanoceramics, both Be 0.1 Mg 0.9 Al 2 O 4 and Be 0.2 Mg 0.8 Al 2 O 4 show transmissions ∼30% lower at wavelength in the infrared range. The samples show a Vickers hardness of ∼19.2 GPa with no apparent dependence on grain size. These values are consistently lower to those reported for beryllium-free MgAl 2 O 4 spinel with similar grain size. 27 Al and 9 Be Nuclear Magnetic Resonance (NMR) spectroscopy reveals that beryllium does not have a significant effect on cationic site inversion in the spinel and, similar to beryllium-free MgAl 2 O 4 , inversion remains solely a function of grain size. The results indicate beryllium ions form solid-solutions with MgAl 2 O 4 spinel structure and do not alter the grain boundaries significantly enough to influence the mechanical properties of nanocrystalline ceramics.
No takes yet. Share an insight, caveat, or question.
Rogers et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: