The activation volume for the high-temperature steady-state creep of high-purity single-crystal indium in the pressure range of 0.8–5.5 kbar has been obtained using the change-of-slope method. The activation volume obtained is 12.0±0.9 cm3/mole, which corresponds to 0.76 atomic volume.