A series of mesoporous titanosilicate TiMCM-41 molecular sieves with variable amounts of framework titanium have been hydrothermally synthesized using H 2 O 2 as a phase stabilizer. Some structurally analogous materials containing framework zirconium (ZrMCM-41), aluminum (AlMCM-41), or only silicon (MCM-41) have also been synthesized. These materials are calcined to decompose the organic structure-directing agent and used as vanadium supports. Vanadium is loaded onto the supports by incipient-wetness impregnation of a dilute (0.001−0.017 M) aqueous vanadyl sulfate solution. The chemical environment of vanadium in these materials is investigated by electron spin resonance and diffuse reflectance ultraviolet−visible spectroscopy. Both techniques reveal that in freshly prepared siliceous MCM-41 or AlMCM-41 with either low or high vanadium loading only mobile vanadyl VO 2+ ions are detected. By contrast, in freshly prepared TiMCM-41 or ZrMCM-41 with low vanadium loading, vanadium exists as monatomically dispersed square-pyramidal VO 2+ ions and tetrahedral V 5+ ions. This indicates that surface titanium or zirconium centers immobilize these vanadium species and promote the oxidation of VO 2+ to V 5+ . Thus, a strong interaction between vanadium and surface titanium or zirconium centers is suggested. As the vanadium loading in TiMCM-41 increases beyond a critical V/Ti ratio of about 0.17, VO 2+ clusters develop, and some square-pyramidal and distorted octahedral V 5+ ions occur simultaneously by additional coordination to water molecules. This suggests that the accumulation of more than two vanadium ions at a single titanium center occurs at higher vanadium loading. Upon calcination and rehydration in moist air, vanadium is completely oxidized to tetrahedral V 5+ when the vanadium loading is below a critical V/Ti ratio of 0.33 or to some square-pyramidal and octahedral V 5+ at higher vanadium loading. Such an increase in the critical V/Ti ratio on calcination suggests that calcination gives rise to a greater dispersion of the surface vanadium species on the wall surfaces of TiMCM-41.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Luan et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: